About This File
Lots of pics...
Just a quick attempt at acid plating on a failed model (split) after a break from it. but it failed because the copper I'm using is of a different grade than it should be and it just goes weird. Still learning here, just dug up my airbrush from 15 years ago and it still works!!! silver coated before electro bath and voltage was probably too high too. Im gonna try brush plating next. Due to the complete contamination of both copper and solution, a decent plate is not possible anymore but ill keep going till I get nothing.
Gonna do a vid/thread later about this but i need to figure out whats going wrong first!