  1. Used the atomic pull method and the printer is now running completely fine! Not that many print hours so the Teflon coupler is still in full working order
  2. Hi guys I can't seem to work out whats going on here with my print. I've levelled my bed a huge amount of times so the first layer has gone down quite well but as the fill starts to go on the printer makes a rough layer over and over again. The photos show the finished print as well as a print that has been taken off mid way through to show how it builds it up. I've been able to get this print to a high standard before as well as on a quick speed but now my printer is loosing its quality. Nozzle temp 210 Bed 70 first layer 20mm/s then 50mm/s 0.1 layer height with 50% fill and a nice 3 line Brim
×
×