Hello,
I'm a new user of this community. We bought an Ultimaker S5 printer on August 2019. Printing with tought PLA is great, but white PLA give an excessive extrusion on external wall. You can see it on picture below. I tried to print slowly from 70 mm to 50 mm per second, and less heater from 210°C to 200°C. The problem disappear not totally. Also cylinder show narrowing on top. How can we solve it, please?
Thanks in advance for you help.