  1. I have a Flashforge Dreamer 3d, printing PLA at 205 degrees for the extruder and 65 for the bed. The first 5 or so layers of all of my prints have a very subtle but strange blobbing and then everything after that is smooth. Any ideas? I've tread leveling not only with the printers leveling but also simplify 3d wizard. I also have retraction set at 2mm. Attached is a picture of too prints up close...notice the first few layers are extra blobby then everything smooths out? Any thoughts or suggestions?
×
×