Hi,
I have an issue when I print PP. As you can see on the pictures there is one side (bottom side) of the print that is a real mess. That area is where the head gets up and down to change position. Is someone ever experiences some similar issues and could help me with this ?
Here are the settings I used:
- fan speed at 75%
- infill density 105%
- build plate temp. 100°C
- printing temp. 230°C
I also tried those settings but got the same result:
- fan speed at 0%
- infill density 125%
- build plate temp. 85°C
- printing temp. 210°C
Thanks