Posted (edited) · Post-processing tricky pingent

Hi community!

I've a challenge (one more! hehee). Make a little pingent with metal looks like. I never tryed coating before. Galvanization is a good deal or it requires high heat material properties? What technique should I look for? My best filament for heat toleration is PLA Tec, up to 110 degrees (at least).

I also have a bronzefill but pingent looks so tiny (0.8mm minimum) and probably it will be hard to polish for a shine finish... but maybe is the best choice!

That's a preview art sended by client (I will change lots of stuffs here). It could goes at maximum 30mm wide

pingente.thumb.jpg.81e714ec5e18dd33edd867fc4f9fae35.jpg

Even if I didn't get this job I would like to know what kind of coating should I try for other aplications and tests ;)

Cheers bros!

pingente.thumb.jpg.81e714ec5e18dd33edd867fc4f9fae35.jpg

Edited by Guest
  • Link to post
    Share on other sites
    • 2 weeks later...
    Posted (edited) · Post-processing tricky pingent

    Galvanisation requires only 30 degrees heat max. And is fairly painless and will achieve a glossy reflective finish with no sanding. However the solution you do it in is corrosive and you need to wear gloves. But you also need a good print to begin with. First choose either nickel or copper to plate with if you want to do it yourself easily or take it to get chromed somewhere else at a cost.

    Edited by Guest
    • Like 1
    Link to post
    Share on other sites
    • 2 weeks later...
    Posted · Post-processing tricky pingent

    Thank you for the feedback.

    I will definitely try nickel, copper and how cost is to get chomed outside.

    By the way I found a great beginner source written by "Enza3D" to anyone looking for post processing tips, Metal Plating (the right name for "metal looks like" :D) is on the bottom of the page:

    https://www.3dhubs.com/knowledge-base/post-processing-fdm-printed-parts#introduction

    For those looking for advanced tips just follow @cloakfiend specially his topic about "Blended PLA with acetone" or something like that... awesome stuff!:p

  • Link to post
    Share on other sites
    • 3 months later...
    Posted · Post-processing tricky pingent

    A bit late, but still: in car tuning shops, they do have spray paints that give a chrome or gold effect (or any other desired colors with mirror-effect, as in christmas balls).

    On Youtube you find a lot of demo videos. Search for "spray on chrome", or "spray paint mirror chrome effect", or similar.

    It seems to consist of cleaning, spraying on an activator, rinsing with water, spraying on chrome, rinsing with water again, spraying on a sealant varnish, rinsing, drying with compressed air. It also seems to work well on flexible materials, even leather.

    For example these:

     

     

    • Like 1
    Link to post
    Share on other sites
    Posted · Post-processing tricky pingent

    Nice, I saw some videos of people in india doing this kind of stuff to statues, I wonder of the coating is conductive?

    In the mean time I'm gonna get some of this and will report back.....

  • Link to post
    Share on other sites
    Posted · Post-processing tricky pingent

    Nice, I saw some videos of people in india doing this kind of stuff to statues, I wonder of the coating is conductive?

    In the mean time I'm gonna get some of this and will report back.....

    Did you check the prices of the setups? Wow....

  • Link to post
    Share on other sites
    Posted · Post-processing tricky pingent

    ...

    I wonder of the coating is conductive?

    ...

    If you would like to try it, maybe you could ask a couple of manufacturers to send a few worthless scrap parts with defects or so, for free? Just to evaluate the surface finish and quality.

    I have also wondered if this is a layer of metal, or metal flakes, chrome powder, or some special optical effect in plastic? But it seems that it has to be covered with a sort of varnish, so probably won't be conductive afterwards.

    I also wondered about scratch-resistance: better or worse than normal paints? The old method in which a shiny chrome layer was put on with vapor, in headlamp mirrors, was extremely weak and susceptible to scratches. You couldn't even wipe it with a soft cloth. But this method seems to be different?

  • Link to post
    Share on other sites
    Posted · Post-processing tricky pingent

    Yeah, I think you can wipe it and stuff after, as I saw them handling the statues and they looked very perfect. But the video was sd, not hd so i can't tell if it covers slight imperfections or anything. The only way to tell is to try it. I kinda though it would be expensive, if its too much, I'll just invest in a larger magnetic stirrer and jug with more copper spate solution and just plate as per normal, at least I know the plating gets thicker the longer i do it so i can't get a nice thick (0.2mm lol) coating easily.

    Ill do a electroplating tut when i have time, been very busy lately.

  • Link to post
    Share on other sites
    Posted · Post-processing tricky pingent
    .....Ill do a electroplating tut when i have time, been very busy lately.

    When you are ready, but I will be looking for that. Some of those paint setups were about 7,000 US. I think the lowest was 2,000 US.

  • Link to post
    Share on other sites
    Posted · Post-processing tricky pingent

    OK so i won't do it then.

    $2000 dollars.... damn, I can buy a hell of a lot of copper with that and copper sulphate. I wonder how much surface area you can cover out of the 2000 bucks? The only problem is storage and stuff, a small setup setup is dirt cheap, so id defo go for that if you've only got small stuff to do. My copper face machine was intended for small rings and stuff ,but I've pretty much dismantled it and plate much larger stuff as you've seen. It definitely takes some getting used to!!! when it doesn't work, its very annoying. The silver spray is also VERY expensive, and the graphite almost useless to plate without experience far cheaper.

  • Link to post
    Share on other sites
    Posted · Post-processing tricky pingent

    Yeah, some of those setups look like some sort of Sci-Fi IV setup for a multitenticled beastie and require a lot of space to spray with a spray booth as well.

    There was one I found a while back that was not nearly as complex. I will have to look for it. Was still expensive though.

  • Link to post
    Share on other sites

    Create an account or sign in to comment

    You need to be a member in order to leave a comment

    Create an account

    Sign up for a new account in our community. It's easy!

    Register a new account

    Sign in

    Already have an account? Sign in here.

    Sign In Now
    • Our picks

      • Ultimaker turns 10: A look back
        Ultimaker is turning 10 years old and that means it is story telling time! We'll explore 2010-2014, traveling through the evolution of the business from the Protobox and Ultimaker Original, to the major leaps forward with the Ultimaker 2 and Ultimaker 3.
          • Like
        • 0 replies
      • Ultimaker Virtual Showroom
        Visit our virtual showroom and learn more about the Ultimaker ecosystem!
        • 15 replies
      • New here? Register your Ultimaker for free 3D printer onboarding course
        Hi,
         
        Often getting started is the most difficult part of any process. A good start sets you up for success and saves you time and energy that could be spent elsewhere. That is why we have a onboarding course ready for
        Ultimaker S5 Pro Bundle, Ultimaker S5, Ultimaker S3 Ultimaker 2+ Connect.   
        They're ready for you on the Ultimaker Academy platform. All you need to do to gain access is to register your product to gain free access. 
        Ready? Register your product here in just 60 seconds.
          • Like
        • 4 replies
    ×
    ×
    • Create New...