  1. but also with pla?

    50mm x 0.2 layer x 0.6 nozzle = 6mm3 , thats 3 times the output volume compared to printing with the standard 0.4 at 0.1 layers.  I would try going up to at least 220 celsius, maybe more.

    there is no "best" temperature, it depends on what you want to achieve. For a strong mechanical part go a bit hotter (=better layer bonding) for a display piece you may want to stay a bit colder, but looking at the fact you use 0.6 + 0.2 layers it's probably not a display piece.

  2. Hi guys,i don't know why i AM not able to print with my um2,it seems like if it wasn't able to extrude enough material,and i print at 50 Speed,0.2 layer, 1.2 shell thichness and 150 of travel Speed,temperature 210,with eumakers pla.i have just changes the ptfe Because i tought that that was the problem but nothing changed....in the pitture is shown the problem....help me please!:(image.thumb.jpeg.4a87855bd566b405143bd73041c1b73f.jpeg

    image.thumb.jpeg.4a87855bd566b405143bd73041c1b73f.jpeg

×
×
  • Create New...