AS REGARDS HEAT-BED: LATELY I HAVE USED FOLLOWING WITH 100% SUCCESS:
NO HEAT-BED
USE PRIMA-BUILDTAK
USED FOR DOZENS PRINTS, EVEN 15 CM HIGH.
FANTASTIC.
USED PLA AT 220C.
-
Just pull out the PLA and cut off the end and push it back again and I have had no problems in a clogged nozzle
Danish / Danmark
in Other Languages
Posted
Er UM-original+ ejer (samlet) siden 2014. Fungere fint. Bruger: PLA 220C; fast; P rime BUILDTAK-helt fint.
Nogle gang maa mand skubber lidt PLA i begyndelsen.
Tempraturen 220 er bedre end 210c.