  1. Hi,

    I am new in 3d printing.

    I got some heavy stringing with one model even with lowering temperature to 190C and increasing travel speed, as shown on picture.

    IMG_1169.thumb.JPG.ab18380d2fd21c3e6831c5924075d3a7.JPG

    After reading about how to minimize it, i set Retraction minimum travel = 0, Enable combing = all,

    Minimal extrusion before retracting = 0 and lowered print speed to 40mm/s.

    I got sliced layers in CURA on attached image. Some of them are pretty clear , but a lot of them still have blue lines

    getting over gaps , some even without retracting.

    Is it possible to force avoiding holes like 100%, because on this model it is possible, and cleaning stringing after pretty impossible? Any suggestions?

    setup cura, i3Hephestos, colorfab PLA

    Thanks