Jump to content

cmd348

Dormant
  • Posts

    3
  • Joined

  • Last visited

Posts posted by cmd348

  1. 5 minutes ago, gr5 said:

    Even on the bottom layer?  By default I think it doesn't reach 100% until the 8th layer.  By then your getting into the "easier" area of the print.


    Thanks gr5,

    I just had a closer look at the cooling settings - full cooling was set a the 5th layer. I’ve changed that to the 2nd layer, keeping the 1st for adhesion. Hopefully this will help.

    -C

    • Like 1
  2. Hey gr5,

    Thanks for the response:

    Regarding overhang - I’m using support starting at 0deg, with Z & X/Y support distance equal to the filament diameter. The rest of the part overhangs came out perfect - just the lower/right-facing surfaces had this issue.

    1) Painters tape is a last option - just spent almost 4K on a UM3 with a heated build plate. I’m looking into dialing in the right settings and get the most out the machine.

    2) My fan speed has always been at 100%. Taking your advice - I’m trying a print now with 60deg on the first layer, 50deg thereafter. I’m also using a glue stick to increase adhesion. I think the heated bed might be the culprit.

    3) Design change is not an option for this part.

    I’ll update once I print the new part. Thanks again.

  3. I’m experience warping on the underside of my parts - see attached images.

    I’m using an Ultimaker 3, printing in PLA with a heated bed, fan cooling, and breakaway support (1+ degrees). Basically default printer/Cura settings.

    Print quality is excellent otherwise. Warping is only present on the underside of the part, nowhere else.

    IMG_8953.JPG

    IMG_8952.JPG

×
×
  • Create New...