Hello everyone,
I'm having some problems with printing Nexeo/DSM Novamid ID 1070 on an Ultimaker S5.
I'm experiencing some warping and bed adhesion issues. My parts warp in the corners and I also see that they partially come loose from the build plate..
I also enlarged the brim a little bit, I might need to make the brim even bigger.
I'm using 3DLac as an adhesive promotor.
I'm using printer settings provided by the supplier (I'll post them below).
I have a document from Nexeo where they give some advice when you are experiencing problems. Unfortunately this a little bit contradictory..
This is what they say:
Warping: Advice is to lower the build plate temperature.. etc.
First layer not sticking/parts coming loose: (amongst other tips) Advice is to raise bed temperature..
This are some of the print settings I use:
Print temperature: 255 °C
Bed temperature: 60 °C
Layer height: 0,2 mm
Should I raise or lower my bed temperature? And are there other tips to make sure my parts come out fine?
Thanks in advance!