I have been getting some "zits" on the outside corner of my print (side facing the prime tower) and was wondering if I need to up my retraction settings or if there are some other settings that would help. I am currently printing using PET+CF with settings of 7.5mm distance, 30mm/s speed. Please let me know!
Thanks, Will
Infinite Material Solutions: Aquasys
in Materials & profiles
Posted · Edited by willryan3
Hello,
I recently got this great (in theory) material that will print with my high temp nylon and can dissolve up to 6x faster than PVA. Since I have been using nylon I know the effects of moisture and dry them out before each trial but it seems I can never get the Aquasys dry enough. I continually have stringing and many problems with it not sticking to layers of itself or layers of the nylon. Again, really great product but am needing some more information on it.
Thanks, Will