UltiMaker uses functional, analytical and tracking cookies. Tracking cookies enhance your experience on our website and may also collect your personal data outside of Ultimaker websites. If you agree with the use of tracking cookies, click “I agree, continue browsing”. You can withdraw your consent at any time. If you do not consent with the use of tracking cookies, click “Refuse”. You can find more information about cookies on our Privacy and Cookie Policy page.
This topic has been a while but I want to share my experience:
I was faced to similar problems, my outer wall didn´`'t connect with the inner wall. I was able to fix this issue a bit more, not perfectly, but acceptable:
Try this:
- increase the infill overlap to at least 30%
- enable ironing to smoothen and connect the outer wall to inner parts:
Since I use this configuration, I had good results by small expenses of increased time and material (around 5-10% ?).
Further settings can be considered:
- printing temperature increase by a few degrees
- decreased print speed
- increase your E-steps for extruding, just a few percent (0,5-1%)
I'm not a professional, but experimenting with above values @213°C print,63°C bed, PLA on glass-bed (no-adhesion additive) had improved my printing quality a lot.
Thin gap between outer wall and inner wall, only on small circular insets but not on the perimeter of the print...
in UltiMaker Cura
Posted
Hi out there !
This topic has been a while but I want to share my experience:
I was faced to similar problems, my outer wall didn´`'t connect with the inner wall. I was able to fix this issue a bit more, not perfectly, but acceptable:
Try this:
- increase the infill overlap to at least 30%
- enable ironing to smoothen and connect the outer wall to inner parts:
Since I use this configuration, I had good results by small expenses of increased time and material (around 5-10% ?).
Further settings can be considered:
- printing temperature increase by a few degrees
- decreased print speed
- increase your E-steps for extruding, just a few percent (0,5-1%)
I'm not a professional, but experimenting with above values @213°C print,63°C bed, PLA on glass-bed (no-adhesion additive) had improved my printing quality a lot.