Hello all
Before I get to my problem, here is the information of the print.
Data:
Printer: Sidewinder X1
Filament is in a dry box with 19 % humidity
Slicing software: Cura
Filament: PETG from 3D Jake 1.75mm
Nozzle 0.4mm
Temp. platform: 75 -80 degrees
Nozzle Temp: 225 degrees
Ventilation off
Print speed 60 mm/s
I have several problems that I can't name but I think the pictures speak a thousand words.
What can I do about this? Thanks already for your help.