Jump to content

Idemaxel

Dormant
  • Posts

    3
  • Joined

  • Last visited

Posts posted by Idemaxel

  1. Thanks for you reaction Yellowshark,

    I use an Ultimaker2 without door. Ambient temperature is around 15°

    All settings are the same as before, I even restored the factory settings to be sure.

    I did not change any fan settings.

    Now I cleaned the printbed with dry paper, that was already better but still the object moved.

    The print bed temperature is 60°

    I do not use any adhesive or spray or tape yet since it worked fin without wit PLA on the glass plate.

    I calibrated the nozzle distance, that must be OK.

    5a3318a0ed3e8_Schermafdruk2016-02-2017_49_20.png.be0351c7671197b521e60e80bc1cd77d.png

    5a3318a0d4b53_Schermafdruk2016-02-2017_49_44.png.8e00438efb6222a5f125cad2b5926a00.png

    I am going to try the Atomic Method. It is very well possible that carbonised material is left because the day before the printer kept printing all night without material...

    Thanks again. I will inform about the result.

    Kind regards

    Axel

    5a3318a0ed3e8_Schermafdruk2016-02-2017_49_20.png.be0351c7671197b521e60e80bc1cd77d.png

    5a3318a0d4b53_Schermafdruk2016-02-2017_49_44.png.8e00438efb6222a5f125cad2b5926a00.png

  2. Hi,

    Could somebody give me a tip concerning PLA material that does not stick anymore on the heated printbed ?

    I printed a lot of things this month, but since yesterday each time the material comes loose from the printbed after a few time.

    I calibrated again, I returned also to the factory settings.

    The troubles began when the PLA filament got trapped and the printer printed all night without material...

    Is my printhead damaged by overheating ?

    Thanks in advance !

    Idemaxel

×
×
  • Create New...