  1. Hello everyone,

     

    I'm having some problems with printing Nexeo/DSM Novamid ID 1070 on an Ultimaker S5. 

    I'm experiencing some warping and bed adhesion issues. My parts warp in the corners and I also see that they partially come loose from the build plate.. 

    I also enlarged the brim a little bit, I might need to make the brim even bigger.

    I'm using 3DLac as an adhesive promotor.

     

    I'm using printer settings provided by the supplier (I'll post them below). 

     

    I have a document from Nexeo where they give some advice when you are experiencing problems. Unfortunately this a little bit contradictory..

     

    This is what they say:

    Warping: Advice is to lower the build plate temperature.. etc. 

     

    First layer not sticking/parts coming loose: (amongst other tips) Advice is to raise bed temperature.. 

     

    This are some of the print settings I use:

    Print temperature: 255 °C

    Bed temperature: 60 °C

    Layer height: 0,2 mm

     

    Should I raise or lower my bed temperature? And are there other tips to make sure my parts come out fine?

     