Hello,
I am using the Ultimaker S5.
I wanted to print with both Novamid ID1030 and Novamid ID1030 CF10.
Didn't try CF10 yet but with ID100 no reinforced, all of my part warp a lot. Can't understand why, I applied Magigoo PA. I put 110°C build plate temperature. Didn't use brim but I really thought I could print without it because I'm doing some test about warpage.
Do you guys have this kind of issue too ? Will I have the same problem with the CF10 ?
Thank you