try 235 nozzle, 70-90 bed (higher temp gives better bed adhesion) and fan 30%
those are the most important settings, you could play with retraction distance (2-7mm) and speed (25-50mm/s)
the petg i use is Verbatim black and even at 180C it stil prints but looses it's gloss and has bad layer adhesion, so it has to shine at least. petg always strings a bit but i love it way better then PLA