UltiMaker uses functional, analytical and tracking cookies. Tracking cookies enhance your experience on our website and may also collect your personal data outside of Ultimaker websites. If you agree with the use of tracking cookies, click “I agree, continue browsing”. You can withdraw your consent at any time. If you do not consent with the use of tracking cookies, click “Refuse”. You can find more information about cookies on our Privacy and Cookie Policy page.
There is a lot better chance of developers seeing this on the GitHub page. If you select "New Issue" you will get an option for a bug report or a "Feature Request".
Have you tried using "Initial Layer Horizontal Expansion" set to a negative number? I usually have it enabled at -0.2mm.
Your build plate temperature can come into play as well.
I have an air-conditioning vent above my printer and I had to print a deflector for it to keep the drafts from affecting prints.
When I print with PETG I must use an adhesion promoter (hairspray in my case) and I often need to add anti-warping tabs to the models or they will lift.
We are happy to announce the next evolution in the UltiMaker 3D printer lineup: the UltiMaker Factor 4 industrial-grade 3D printer, designed to take manufacturing to new levels of efficiency and reliability. Factor 4 is an end-to-end 3D printing solution for light industrial applications
Cura 5.7 is here and it brings a handy new workflow improvement when using Thingiverse and Cura together, as well as additional capabilities for Method series printers, and a powerful way of sharing print settings using new printer-agnostic project files! Read on to find out about all of these improvements and more.
Recommended Posts
GregValiant 1,319
There is a lot better chance of developers seeing this on the GitHub page. If you select "New Issue" you will get an option for a bug report or a "Feature Request".
Have you tried using "Initial Layer Horizontal Expansion" set to a negative number? I usually have it enabled at -0.2mm.
Your build plate temperature can come into play as well.
I have an air-conditioning vent above my printer and I had to print a deflector for it to keep the drafts from affecting prints.
When I print with PETG I must use an adhesion promoter (hairspray in my case) and I often need to add anti-warping tabs to the models or they will lift.