20 minutes ago, Smithy said:You could try a higher temperature. Not sure what UM suggests for drying their PVA, but I think it was something about 70°C.
UM PVA can be dried well over night, so maybe your brand is not the best one, but I don't know Gizmodorks.
I thought about that, higher temp=faster moisture removal. But I wasn't sure if that would damage the PVA. I saw a guide from UM about drying it out on the buildplate and they said to do 55°C. However, they recommend drying for a measly 2 hours.
I suppose I could drying it again. 🤷♂️ Just keep measuring the weight until it stabilizes.
Recommended Posts
Smithy 1,146
You could try a higher temperature. Not sure what UM suggests for drying their PVA, but I think it was something about 70°C.
UM PVA can be dried well over night, so maybe your brand is not the best one, but I don't know Gizmodorks.
Link to post
Share on other sites