joergen 2
ABS will always have the tendency to curl up in the corners. I would use a large brim, or at least manual pads on the corners. this will allow for a larger area to hold down your print, and prevent cool air from getting under the corner, which will also increase the curling.
As a side note, the glass-transition temperature of ABS is around 110C, this is when ABS becomes solid.
if your HBP is at 145C (actual, not what you are measuring), your print has no chance of solidifying, and will probably be a wobbly mess.